Enhanced growth and photoluminescence properties of SnxN y (x>y) nanowires grown by halide chemical vapor deposition
(2011)Tin nitride nanowires have been grown by halide chemical vapor deposition via the reaction of Sn with NH4Cl at 425 °C under a steady flow of NH3 using small ramp rates y) with a hexagonal structure, i.e. c=5.193 , a=3.725 ...
-
Article
Enhanced growth and photoluminescence properties of SnxN y (x>y) nanowires grown by halide chemical vapor deposition
(2011)Tin nitride nanowires have been grown by halide chemical vapor deposition via the reaction of Sn with NH4Cl at 425 °C under a steady flow of NH3 using small ramp rates y) with a hexagonal structure, i.e. c=5.193 , a=3.725 ...
-
Article
Hydride-assisted growth of GaN nanowires on Au/Si(0 0 1) via the reaction of Ga with NH3 and H2
(2010)High quality, straight GaN nanowires (NWs) with diameters of 50 nm and lengths up to 3 μm have been grown on Si(0 0 1) using Au as a catalyst and the direct reaction of Ga with NH3 and N2:H2 at 900 °C. These exhibited ...
-
Article
Hydride-assisted growth of GaN nanowires on Au/Si(0 0 1) via the reaction of Ga with NH3 and H2
(2010)High quality, straight GaN nanowires (NWs) with diameters of 50 nm and lengths up to 3 μm have been grown on Si(0 0 1) using Au as a catalyst and the direct reaction of Ga with NH3 and N2:H2 at 900 °C. These exhibited ...
-
Article
A systematic study of the nitridation of SnO 2 nanowires grown by the vapor liquid solid mechanism
(2012)SnO 2 nanowires (NWs) with diameters of 50 nm and lengths ≥10 μm have been grown at 800 °C on 1.0 nm Au/Si(001) via the vapor liquid solid mechanism and the low pressure chemical vapor deposition. These exhibited clear ...
-
Article
A systematic study of the nitridation of SnO 2 nanowires grown by the vapor liquid solid mechanism
(2012)SnO 2 nanowires (NWs) with diameters of 50 nm and lengths ≥10 μm have been grown at 800 °C on 1.0 nm Au/Si(001) via the vapor liquid solid mechanism and the low pressure chemical vapor deposition. These exhibited clear ...