Adaptive VN/Ag nanocomposite coatings with lubricious behavior from 25 to 1000 °c
(2010)
A two-phase nanocomposite coating that consists of inclusions of silver in a vanadium nitride matrix (VN/Ag) was investigated as a potential adaptive coating with a reduced friction coefficient from 25 to 1000 °C. This ...
Textured VN coatings with Ag3VO4 solid lubricant reservoirs
(2011)
Silver oxovanadate powders were produced using a low temperature hydrothermal synthesis method. X-ray diffraction (XRD) and Raman microscopy revealed the formation of the α-Ag3VO4 phase, and differential scanning calorimetry ...
Effect of silicon nitride/oxide on the structure and the thermal conductivity of CoSi nanocomposites
(2017)
In this work, the fabrication of nanocomposites with silicon nitride/oxide into the thermoelectric matrix of cobalt silicide is presented. The different concentrations of nano-Si3N4 were intentionally introduced by mechanical ...
Few-step synthesis, thermal purification and structural characterization of porous boron nitride nanoplatelets
(2016)
Hexagonal boron nitride (h-BN) nanoplatelets with 99 wt.% purity, 900 to 2000 nm particle width, 30 to 90 nm particle thickness, 213 m2/g specific surface area (SSA), 66% micropore SSA and 0.85 nm average pore size were ...
Thermal and chemical stability of hexagonal boron nitride (h-BN) nanoplatelets
(2015)
High-temperature properties of boron nitride platelets (200-800 nm in width and 30-50 nm in thickness) were systematically evaluated through thermogravimetric analysis (TGA) in combination with differential scanning ...
A systematic study of the nitridation of SnO 2 nanowires grown by the vapor liquid solid mechanism
(2012)
SnO 2 nanowires (NWs) with diameters of 50 nm and lengths ≥10 μm have been grown at 800 °C on 1.0 nm Au/Si(001) via the vapor liquid solid mechanism and the low pressure chemical vapor deposition. These exhibited clear ...
The nitridation of ZnO nanowires
(2012)
ZnO nanowires (NWs) with diameters of 50 to 250 nm and lengths of several micrometres have been grown by reactive vapour transport via the reaction of Zn with oxygen on 1 nm Au/Si(001) at 550°C under an inert flow of Ar. ...
Enhanced growth and photoluminescence properties of SnxN y (x>y) nanowires grown by halide chemical vapor deposition
(2011)
Tin nitride nanowires have been grown by halide chemical vapor deposition via the reaction of Sn with NH4Cl at 425 °C under a steady flow of NH3 using small ramp rates y) with a hexagonal structure, i.e. c=5.193 , a=3.725 ...